Daylight Precision Castable Violet Resin | 1Kg

78.00 €
Tax excluded
Not Rated
fai acquisti fino a 3.000€ e paga in 3 rate con  paga a rate Klarna
buy up to €3.000 and pay in 3 with  pay in 3 with Klarna
prodotto presente su  Crea3D è presente su MEPA

Volume discounts

QuantityPriceYou Save
374.10 €Up to 11.70 €
670.20 €Up to 46.80 €
1266.30 €Up to 140.40 €
Delivery 15 business days

 

Daylight Precision Castable Violet Resin

For creating highly accurate jewellery parts for investment casting, use our Cast resin. Printed parts display high accuracy and detail which shows in the smooth, crisp finish on the cast parts. Virtually no ash or residue, no expansion, and highly detailed parts can be obtained using Cast.

 

Precision Cast has been designed for creating high definition castable parts especially for the Precision Printer.
The printed parts will display a high accuracy and detail for the use in the modern jewellery market.
This product has been formulated to burn evenly to reduce gas pressure in the cast and leave virtually no ash or residues (Please refer to our casting guidelines).
The parts printed with this resin will have virtually no expansion.
The cast parts will display a smooth surface and a good surface finish.

Key benefits include a reduced ash and residue content in burnout, no expansion when heated, highly accurate printed parts with a good smooth surface finish, highly accurate metal cast parts with a good surface finish.

PRECBVI01
Color Violet
Viscosity
(At 25ºC Brookfield spindle 3)
630 cPs
Hardness
ASTM D2240 (After post exposure, 1hr UV)
75 Shore D
Tensile strength
ASTM D638 (After Post Exposure, 1hr UV)
19.5 MPa
Tensile strength
ASTM D638 (Before Post Exposure)
10 MPa
Tensile modulus
 ASTM D638 (After Post Exposure, 1hr UV)
1380 MPa
Elongation at break
ASTM D638 (After Post Exposure)
2-3%
Storage 1050°C
Density 1.20 g/cm3

 

Processing Instructions

Follow the procedures laid out in your 3D Precision ́s user manual.
Polymer should be poured into the tray away from direct sunlight and after being shaken for two minutes.
It is important to mix well the resin in the tray with the card provided before starting the print.
Polymer can be reused but should be poured through a filter to remove solid lumps. Keep hood on at all times.

First rinse with warm water, then spray with Photocentric Resin Cleaner (recommended), alternatively IPA or acetone can be used. Then rinse with warm water again. Drying your parts with an air gun will help ensure all holes and slots are open, if present.

Place the parts in an oven at 120 °C for 4 hours: surfaces should be tack free.
If still tacky, return items to the oven. As this resin contains a concentration of wax there is the chance that wax separation may occur in unpredictable climates.
To solve this issue, we advise warming up the resin to around 50 °C and then shaking this will re-incorporate the solid layer